Clear the cavity and reinstate trays
Cavity walls only work if the cavity is clear and trays shed water at openings, abutments, and changes in construction. Mortar droppings and debris bridge the cavity and take rain to the inner leaf.
The mechanism is well described, and this is the repair set out in a British Standard, an Approved Document, BRE guidance, or equivalent mainstream practice. It still has to match the building in front of you.
When it works
Rain is crossing at a bridge: above a window, at a roof abutment, or where debris has filled the cavity at the base. The repair is local and is confirmed by looking, not by injecting the inner leaf.
When it fails or causes harm
The cavity is doing its job and the mark is condensation on a cold inner leaf. Do not open a sound cavity as a ritual.
Frequently asked
When should cavity trays and weep clearance be reinstated rather than injecting a DPC?
Whenever rain is crossing at a cavity bridge — above openings, at roof abutments, or where mortar debris fills the cavity base — and the stain is weather-timed on a cavity wall (BS 8104 / Approved Document C). The repair is local: clear droppings, reinstate trays with stop-ends, and open weeps so water sheds out. Injecting the inner leaf does not recreate a tray and leaves the bridge in place (BRE Digest 245 logic on bridging vs course failure). Look into the cavity before naming rising damp; do not open a sound cavity as ritual when the mark is condensation on a cold inner leaf.