Defects
Defects
Damp, mould, movement, materials failure, and biological attack — with checks that help you tell likely causes apart, including notes for other climates and regions.
How to use this section. Topics are grouped by type of failure — damp, mould, movement, materials, and biological attack. Each topic explains how that cause works and what checks help tell causes apart. Notes for other climates and regions are included where practice differs.
Frequently asked
What diagnostic sequence should a surveyor follow before naming a damp mechanism?
Order before product. (1) Ask what changed — new windows, cavity fill, raised patio, blocked air bricks, a gutter failure, clothes dried indoors — because damp that started after a change is naming the change. (2) Name the construction before any remedy: solid brick/stone, early cavity, insulated cavity, timber frame, slab or suspended floor; brick slips and stud partitions cannot have rising damp. (3) Map pattern on paper: height, elevation, rain vs cold weather vs humidity, chimney/gutter/pipe alignment; photograph with a scale. (4) Read the outside first — Approved Document C clearance (~150 mm ground to DPC), gutters that run, open joints, trays, weeps, air bricks. (5) Distrust the conductance meter: BRE Digest 245 — a high reading is not rising damp; where money will be spent, use oven-dried drilled samples separating free and hygroscopic moisture (BS 6576 context). (6) Name the mechanism only when confirm/falsify tests fit; if two still fit, buy the separating observation, not a ‘safe’ injection. Write construction, observations, leading mechanism, falsifiers, and the evidence grade of any repair. BS 5250 frames moisture risk; do not tank a lime wall or inject a condensating bedroom to be thorough.
Outside the UK
The physical causes are the same worldwide; which ones are likely depends on how the building is put together. Tropical AC reverse condensation, termites, and RC corrosion already have dedicated records. For how these show up on US timber frames, in Southeast Asia, and on hot-arid walls, open defects in other regions.
Moisture
- Surface condensationRoom air meeting a cold surface, dropping water, and often growing black mould. It is the most common damp mis-sold as rising damp.
- Condensation inside the wall or roof layers (interstitial condensation)Water condensing inside the construction, not on the paint. Typical of cold roofs, timber frames with a broken vapour-control layer (on the warm side of the wall), and solid walls insulated on the inside without a moisture assessment.
- Penetrating dampRain getting through the envelope (the outside walls and roof): open joints, cracked render, failed trays, a bridged cavity, or a solid wall in driving rain that can no longer dry.
- Rising damp and a bridged damp-proof courseGround moisture held in the base of a masonry wall. Genuine capillary rise (moisture climbing from the ground through the masonry) happens. It is diagnosed far more often than it is present. A bridged damp-proof course is the usual real version.
- Hygroscopic salts (salts that draw damp from the air)Salts already in the plaster or masonry pull moisture out of humid air. The patch returns in muggy weather even when the leak or the ground water has stopped.
- A leak from a pipe, a roof, or a fittingLiquid water from a failed pipe, a flat roof, a valley, a flashing, or an air-conditioner condensate. It is ordinary until it is called rising damp.
- Moisture and decay under a timber ground floorA suspended timber floor with a wet, still void after designed air-brick airflow was blocked. Joists, wall plates, and ends built into the wall decay; ground-floor damp is often mis-sold as rising damp.
- Spray foam insulation on pitched roof rafters (trapped moisture & rot)Closed-cell or open-cell polyurethane foam sprayed directly against the underside of roof slates/tiles or timber rafters, blocking ventilation paths, trapping condensation, causing rafter rot, and triggering mortgage retentions.
- Flat roof ponding & cold-deck deck condensationRainwater standing in pools >48 hours due to inadequate structural falls (< 1:80), combined with cold-deck vapour condensation that rots the structural timber deck from beneath.
- Missing or defective cavity trays at pitched roof abutmentsRain penetrating the external brick leaf above a single-storey lean-to extension or conservatory running down inside the cavity and soaking internal ceilings because stepped cavity trays were omitted.
- Tropical reverse condensation from indoor air conditioningIn hot-humid Southeast Asia, cooling bedrooms to 20°C–22°C causes hot external air (35°C, 85% RH) to drive water vapour inward, creating hidden condensation traps behind impervious wallcoverings.
- Window and door installation defectsRain and draughts at openings caused by poor fixing, missing cavity closers/trays, failed sealants, and bridges at sills — not ‘the window product failed’ as a first story.
- Basement and cellar groundwater ingressWater and damp below ground level from hydrostatic pressure, failed tanking, neglected drained cavities, or a cellar never designed as a dry room.
- Thermal bridging and cold spotsLocal heat loss at junctions, lintels, slab edges, and fixings that cool the inner surface below dew point — mould without a ‘damp course’ story.
- EWI and thick-render moisture trapsRain and vapour trapped at failed EWI junctions, cracked render, buried DPCs, and sealed reveals after external insulation or thick modern render.
- Podium deck and green-roof waterproofing failureLeaks through landscaped decks and green roofs into rooms or car parks below — membrane breaches, blocked drainage, and penetrations.
- Cavity wall insulation failure and bridgingBead, fibre, or foam cavity fills that bridge the cavity, hold water against the inner leaf, or were installed into dirty/ bridged cavities — rain and cold spots after ‘energy upgrade’.
- Central heating and hot-water cylinder leaksWater damage from heating pipework, radiators, valves, and hot-water cylinders — often misread as roof or rising damp when the stain is service-fed.
- EIFS and rainscreen water intrusion (North America)Water behind exterior insulation and finish systems (EIFS) and similar cladding — missing drainage planes, flashings, and sealant failures that wet sheathing and framing.
- Slab-edge damp and termite risk at ground junctionsMoisture and pest paths at ground-bearing slab edges, rebates, and landscaping build-ups — including Australian and other warm-climate termite inspection zones at the perimeter.
- Balcony waterproofing and threshold failuresLeaks at balcony decks, door thresholds, and upstands — beyond a single missing cavity tray — where membranes, falls, and drainage meet the living space.
- Chimney stack decay and flue condensationRain and condensate attacking unused or partially used chimney stacks — sulphate attack, staining, and wet breasts mis-sold as rising damp.
- Parapet and abutment weathering failuresRain entry at parapets, copings, and roof abutments where flashings, trays, and weathered masonry meet — distinct from mid-span flat-roof ponding alone.
- Conservatory and orangery thermal-break failuresCondensation, mould, and cold floors where lightweight glazed rooms meet the heated house without adequate thermal breaks, drainage, and vapour control.
Structure and movement
- Cavity wall tie corrosionSteel ties in early cavity walls rust, expand, crack the bed joints, and stop tying the two leaves. In a high wind that can be more than a crack.
- SubsidenceThe ground under part of the building goes down, and the building follows. Clay shrinkage, leaking drains, and weak or eroded ground are the usual domestic causes. It is not the same as a crack.
- SettlementThe building or its fill compressing soon after it was built, then usually stopping. Old, stable settlement is a record, not a live defect.
- HeaveClay swelling and lifting part of the building, commonly after a tree is removed or after a dry period ends. The opposite of shrinkage subsidence, and often caused by the attempt to cure it.
- Movement between a frame and its infillThe concrete frame and the brick or block panel are different materials. They shrink, creep, and move with temperature at different rates. The crack follows the joint between them.
Materials
- A coating the wall cannot breathe throughCement render, hard cement pointing, or a waterproof coating on a solid wall that was built to dry. The face spalls, salts build up, and the inside gets wetter.
- Corrosion of reinforcementSteel in concrete rusts, expands, and spalls the cover. Thin cover, carbonation, and salt near the coast are the usual reasons. A skim of plaster over the rust is not a repair.