Defect · materials
Corrosion of reinforcement
Steel in concrete rusts, expands, and spalls the cover. Thin cover, carbonation, and salt near the coast are the usual reasons. A skim of plaster over the rust is not a repair.
Mechanism
Concrete protects steel because the pore water is alkaline. Carbon dioxide slowly carbonates that cover from the outside in. When the front reaches the bar, or when chlorides from the sea or from contaminated aggregates arrive sooner, the steel corrodes. The rust splits the concrete along the bar. You see rust stains, cracks in line with the steel, and eventually exposed bars. It is common in older concrete frames in warm humid climates, and in lintols, balconies, and some system-built panels in England. The repair removes unsound concrete, treats the bar, and puts back a cover designed for the exposure.
Often confused with
- Infill cracking at the edge of a concrete column, where the brick meets the frame and there is no rust
- Wall-tie corrosion in a brick cavity wall
- Paint stains that look like rust
What would support it
- Cracks and spalls in line with the reinforcement, rust staining, exposed steel
- Low cover measured, or a marine or de-icing exposure
- An engineer checking whether the bar has lost section, not only whether it looks untidy
What would rule it out
- The crack is exactly at the junction of infill and frame, the concrete arris is intact, and there is no rust
- The building is unreinforced masonry
Common mistakes to avoid
- Do not paint the rust and skim it
- Do not call every crack in a concrete frame 'concrete cancer'
Remedies
- EstablishedRepair corroding reinforcement
Spalling concrete with rust stains is steel expanding as it corrodes, usually because cover was thin or carbonation and chlorides have reached the bar. The repair cuts back to sound steel, cleans it, and reinstates cover in a system meant for the exposure.
- EstablishedRecord cracks properly
Tell-tales, dated photographs with a scale, and a note of doors that stick. Digest 251 asks what repair the damage would need, not merely how wide one crack is. A single visit cannot show whether movement has stopped.