Houses built from a named system: precast concrete panels, concrete columns, steel frames, and others. Some prefabricated reinforced-concrete systems are designated defective under the Housing Act 1985. The name of the system comes before any opinion.

Mostly 1940s to 1960s

How to recognise it

  • Panel joints, bolt heads, distinctive column profiles, or a steel frame at the eaves. Pebbledash on its own identifies nothing
  • Airey houses have reinforced concrete columns at close centres. BISF is a steel frame with a different repair history and is not that PRC list
  • Local authority and lender records, and someone who has surveyed the type, beat a guess from the pavement

How it is built

  • Each system has its own frame, panel, and joint. The joint is usually where rain gets in
  • Designation under the Housing Act is a statutory list of named PRC systems. It affects history and lending. It is not a description of every non-traditional house
  • Repairs, where they exist, are system-specific. A generic cavity-wall detail does not apply

How it behaves

Carbonation of poorly covered reinforcement, corrosion of steel, and leaking panel joints are the recurring themes. Condensation happens for the same physical reasons as anywhere, often worse because the walls are cold and the joints are thermal bridges. This record exists so an agent does not treat a named system as 'a kind of brick cavity'. It is not a schedule of repairs for each system.

What to watch

  • Any advice, including from this site, that names a repair before the system is identified
  • Panel joints opened by movement and left unsealed
  • Reinforcement corrosion passed off as ordinary render cracking

Mechanisms that belong here

  • Surface condensation

    Room air meeting a cold surface, dropping water, and often growing black mould. It is the most common damp mis-sold as rising damp.

  • Penetrating damp

    Rain getting through the envelope (the outside walls and roof): open joints, cracked render, failed trays, a bridged cavity, or a solid wall in driving rain that can no longer dry.

  • Rising damp and a bridged damp-proof course

    Ground moisture held in the base of a masonry wall. Genuine capillary rise (moisture climbing from the ground through the masonry) happens. It is diagnosed far more often than it is present. A bridged damp-proof course is the usual real version.

  • Hygroscopic salts (salts that draw damp from the air)

    Salts already in the plaster or masonry pull moisture out of humid air. The patch returns in muggy weather even when the leak or the ground water has stopped.

  • A leak from a pipe, a roof, or a fitting

    Liquid water from a failed pipe, a flat roof, a valley, a flashing, or an air-conditioner condensate. It is ordinary until it is called rising damp.

  • Subsidence

    The ground under part of the building goes down, and the building follows. Clay shrinkage, leaking drains, and weak or eroded ground are the usual domestic causes. It is not the same as a crack.

  • Settlement

    The building or its fill compressing soon after it was built, then usually stopping. Old, stable settlement is a record, not a live defect.

  • Heave

    Clay swelling and lifting part of the building, commonly after a tree is removed or after a dry period ends. The opposite of shrinkage subsidence, and often caused by the attempt to cure it.

  • Corrosion of reinforcement

    Steel in concrete rusts, expands, and spalls the cover. Thin cover, carbonation, and salt near the coast are the usual reasons. A skim of plaster over the rust is not a repair.

  • Movement between a frame and its infill

    The concrete frame and the brick or block panel are different materials. They shrink, creep, and move with temperature at different rates. The crack follows the joint between them.