Concrete block walls

Dense or aircrete blocks. As the inner leaf of a cavity they are ordinary. As a single leaf — garages, rear extensions, boundary walls, some whole houses — they have no cavity, they crack at changes of construction, and rain goes through the joints.

Throughout the twentieth century, and still the inner leaf of cavities

How to recognise it

  • Block sizes and a rendered or painted face. Aircrete (Thermalite, Celcon and similar) is light and easy to dent; dense aggregate block is heavier and harder
  • A single-leaf extension often shows a straight joint against the original house, with a different thickness
  • Do not confuse the inner leaf of a cavity, which you only see from inside, with a single-leaf external wall

How it is built

  • Typically 100 mm single leaf for garages and cheap extensions, rendered or fair-faced
  • Aircrete is thermally better and weaker at holding fixings. It is damaged by prolonged wetting and frost
  • Lintels over openings are often concrete and can corrode if the cover is poor

How it behaves

A single leaf relies on the render or the paint and the joints to shed rain. Cracks at the junction with the house, at the lintel, and at long unjointed runs let water in, and a cold single leaf condensates freely. A damp-proof course is frequently bridged by the path outside a garage or extension. Where the block is only the inner leaf, diagnose the cavity wall, not the block.

What to watch

  • Cracks at the junction with the original building
  • Paint and render treated as a damp-proof course
  • Aircrete soaked by a planter built against it
  • Undersized lintels and corroding concrete lintels

Frequently asked

How does concrete blockwork behave for moisture compared with solid brick?

As a cavity inner leaf, diagnose the cavity system, not the block. As a single leaf (garages, cheap extensions), there is no cavity break — rain enters at cracked render/joints and cold faces condensate freely (BS 5250). Aircrete is lighter and more vulnerable to prolonged wetting/frost; dense aggregate is harder but still joint-dependent. Bridging of the DPC by paths and plaster follows the same Approved Document C / BRE Digest 245 rules as brick. Single-leaf block needs intact weather face and movement detailing at junctions with the host house; do not specify lime-breathability slogans meant for Victorian brick onto a cement-rendered 100 mm garage leaf without checking the actual build-up.

Mechanisms that belong here

  • Surface condensation

    Room air meeting a cold surface, dropping water, and often growing black mould. It is the most common damp mis-sold as rising damp.

  • Penetrating damp

    Rain getting through the envelope (the outside walls and roof): open joints, cracked render, failed trays, a bridged cavity, or a solid wall in driving rain that can no longer dry.

  • Rising damp and a bridged damp-proof course

    Ground moisture held in the base of a masonry wall. Genuine capillary rise (moisture climbing from the ground through the masonry) happens. It is diagnosed far more often than it is present. A bridged damp-proof course is the usual real version.

  • Hygroscopic salts (salts that draw damp from the air)

    Salts already in the plaster or masonry pull moisture out of humid air. The patch returns in muggy weather even when the leak or the ground water has stopped.

  • A leak from a pipe, a roof, or a fitting

    Liquid water from a failed pipe, a flat roof, a valley, a flashing, or an air-conditioner condensate. It is ordinary until it is called rising damp.

  • A coating the wall cannot breathe through

    Cement render, hard cement pointing, or a waterproof coating on a solid wall that was built to dry. The face spalls, salts build up, and the inside gets wetter.

  • Subsidence

    The ground under part of the building goes down, and the building follows. Clay shrinkage, leaking drains, and weak or eroded ground are the usual domestic causes. It is not the same as a crack.

  • Settlement

    The building or its fill compressing soon after it was built, then usually stopping. Old, stable settlement is a record, not a live defect.

  • Heave

    Clay swelling and lifting part of the building, commonly after a tree is removed or after a dry period ends. The opposite of shrinkage subsidence, and often caused by the attempt to cure it.

  • Corrosion of reinforcement

    Steel in concrete rusts, expands, and spalls the cover. Thin cover, carbonation, and salt near the coast are the usual reasons. A skim of plaster over the rust is not a repair.