UK & Ireland · Walls
No-fines concrete
Cast concrete made without fine aggregate, usually rendered. It is not the same thing as a designated prefabricated reinforced-concrete system. It has its own cracking, render, and reinforcement details.
Mostly 1940s to 1970s, including Wimpey No-Fines
How to recognise it
- A rendered, often pebbledashed house of the post-war decades, with a heavy solid feel and no brick bond
- Identification is not something to do from a sales particular. No-fines, Airey, and other systems can all wear pebbledash
- Corners, ring beams, and lintels may contain ordinary reinforced concrete even when the wall is no-fines
How it is built
- Poured no-fines concrete in shutters, generally two storeys, with a render coat that is doing the weather protection
- The no-fines mass is relatively permeable. The render is the raincoat
- Wimpey No-Fines is the best-known system. It is not on the list of PRC systems designated under the Housing Act in the way Airey, Orlit, or Unity are
How it behaves
If the render cracks, rain goes into a porous wall and shows inside. That is penetrating damp, repaired at the render and the joints, not by a damp-proof course slogan. Reinforcement at lintels and beams can corrode where cover is poor. Cracking needs the same discipline as any other house: cause, not a label. Mortgage comments should follow a proper identification, not this paragraph.
What to watch
- Calling it a designated PRC house without naming the system
- Cracked render left as a 'feature of the type'
- Corroding steel at lintels and ring beams
- Cement coatings that trap water in the no-fines
Frequently asked
How do no-fines and other system-built houses change the defect shortlist?
No-fines (e.g. Wimpey) is permeable mass behind a render raincoat — cracked render equals penetrating damp, not a Victorian DPC story; reinforcement at lintels/ring beams can corrode (BS EN 1504 context). Designated PRC and other named systems (Airey, Orlit, Unity, etc.) add panel joints, carbonation, and system-specific repairs under Housing Act designation history — still not ‘a kind of brick cavity’. Condensation remains BS 5250 physics on cold panels. Identify the system before any repair list; pebbledash alone names nothing. Do not paste cavity-tray or chemical-DPC details onto an unidentified non-traditional house.
Mechanisms that belong here
- Surface condensation
Room air meeting a cold surface, dropping water, and often growing black mould. It is the most common damp mis-sold as rising damp.
- Condensation inside the wall or roof layers (interstitial condensation)
Water condensing inside the construction, not on the paint. Typical of cold roofs, timber frames with a broken vapour-control layer (on the warm side of the wall), and solid walls insulated on the inside without a moisture assessment.
- Penetrating damp
Rain getting through the envelope (the outside walls and roof): open joints, cracked render, failed trays, a bridged cavity, or a solid wall in driving rain that can no longer dry.
- Rising damp and a bridged damp-proof course
Ground moisture held in the base of a masonry wall. Genuine capillary rise (moisture climbing from the ground through the masonry) happens. It is diagnosed far more often than it is present. A bridged damp-proof course is the usual real version.
- Hygroscopic salts (salts that draw damp from the air)
Salts already in the plaster or masonry pull moisture out of humid air. The patch returns in muggy weather even when the leak or the ground water has stopped.
- A leak from a pipe, a roof, or a fitting
Liquid water from a failed pipe, a flat roof, a valley, a flashing, or an air-conditioner condensate. It is ordinary until it is called rising damp.
- A coating the wall cannot breathe through
Cement render, hard cement pointing, or a waterproof coating on a solid wall that was built to dry. The face spalls, salts build up, and the inside gets wetter.
- Subsidence
The ground under part of the building goes down, and the building follows. Clay shrinkage, leaking drains, and weak or eroded ground are the usual domestic causes. It is not the same as a crack.
- Settlement
The building or its fill compressing soon after it was built, then usually stopping. Old, stable settlement is a record, not a live defect.
- Heave
Clay swelling and lifting part of the building, commonly after a tree is removed or after a dry period ends. The opposite of shrinkage subsidence, and often caused by the attempt to cure it.
- Corrosion of reinforcement
Steel in concrete rusts, expands, and spalls the cover. Thin cover, carbonation, and salt near the coast are the usual reasons. A skim of plaster over the rust is not a repair.